AquaSys 180

Infinite Material Solutions
SKU: 811175500G
$200.00
AquaSys® 180 is the world’s only water-soluble 3D printing support material that’s compatible with Polyetheretherketone (PEEK), Polyetherketoneketone (PEKK), Polyetherimide (PEI), and polyphenylsulfone (PPSU).

It’s stable at chamber temperatures up to 180ºC. It provides complete design freedom. And it allows the additive manufacturing industry to move on to its next frontier: printing complex end-use parts, using high-strength thermoplastics.

At Vision Miner, we use Aquasys 180 with PEEK, ULTEM, and other materials on the AON-M2, Funmat Pro 410, and other experimental machines -- it's incredible to have soluble supports for the high-temps, finally!

QTY:


 

Details

Want a closer look at what makes AquaSys® 180 effective and safe
to work with? Get more critical details by downloading the
Technical and Safety Data Sheets (TDS & SDS).

DOWNLOAD SDS

DOWNLOAD TDS

DOWNLOAD WHITEPAPER


Specifications


  • Diameter: 1.75mm
  • Volume: 500g
  • Extruder temperature: 230-300ºC (240-260ºC recommended)
  • Build plate temperature: 60-180ºC
  • Chamber temperature: Up to 180ºC
  • Bed Adhesive: Nano Polymer Adhesive


Compatibility


AquaSys® 180 is engineered for enhanced adhesion and high thermal stability. Together, these properties allow it to bond effectively to a wide range of hydrophobic and hydrophilic materials. And while it does adhere to most commonly used 3D printing materials, it’s recommended primarily for use with PEEK, PEKK, PEI, and PPSU.

Working with lower temperature materials like ABS or PP? Try AquaSys ®120.

Printer Compatibility

AquaSys® 180 filament is designed for use in fused filament fabrication (FFF) printers.

Printing Parameters

  • Pathway temperature: Keep the filament below 80°C prior to extrusion. Material that sits idle at temperatures of 80°C or above for extended periods of time prior to extrusion will not extrude properly.
  • Nozzle temperature: 230 - 300°C
  • Build plate requirements: AquaSys filaments will adhere to a wide range of build plate materials. If poor adhesion is persistent, increase the temperature of the build plate, but not past the maximum build plate temperature of 180°C.

Pair AquaSys 180 with any of the following: PEEK, PEKK, PEI, PPSU, CFPEEK, and more.